Ancordent Dental Laser Welding Wire 0.50 mm – 2 m Roll
Référence: H04400
Ancordent laser welding wire – 0.50 mm – 2 m roll
Professional wire for laser welding of dental alloys
In a dental laboratory, technicians frequently need to carry out repairs or additions that require high mechanical strength. The Ancordent laser welding wire in roll form allows you to work on:
- CoCr frameworks.
- Implant bars.
- Clasps and prosthetic frameworks.
- Orthodontic components.
Its stable metallic behaviour ensures clean fusion, a reduced heat-affected zone and excellent reliability in the laboratory.
Key advantages of laser welding in dental prosthetics
- Extreme precision: laser welding heats only the targeted area, enabling highly localised repairs or additions without deforming the framework.
- Very small heat-affected zone: preserves resin teeth, composite teeth, ceramics and adjacent acrylic parts.
- High mechanical strength: welded joints provide strength comparable to the original alloy.
- No soldering alloy required: direct welding avoids brittle solder alloys and improves toughness and biocompatibility.
- Ideal for delicate repairs: clasp modification, local reinforcement, framework extension, repair of cracks without complete disassembly.
- Compatible with most dental alloys: CoCr and other alloys suitable for laser welding.
- Homogeneous fusion: the filler metal integrates with minimal porosity, ensuring a clean and durable result.
- Improved productivity: welding operations are fast and do not require long thermal cycles.
Applications in the dental laboratory
- Fast repair of metal frameworks or fractured prosthetic frameworks.
- Adjustments and extensions of CoCr clasps without damaging resin areas.
- Assembly of bars or reinforcements on fixed or removable prostheses.
- Modification of weakened or cracked connectors.
- Adding attachment points, local reinforcement, small metal build-ups and metal attachments.
Instructions for use (general recommendations)
- Thoroughly clean the area to be welded (fine sandblasting or steam cleaning).
- Prepare a fresh metal surface to ensure optimal fusion.
- Use short lengths of filler wire to avoid excessive build-up.
- Perform welding with short pulses to limit heat diffusion.
- Visually check fusion: the metal must blend homogeneously.
- Deburr and polish after cooling, if necessary.
Technical specifications
| Feature | Value |
|---|---|
| Brand | Ancordent |
| SKU | H04404 |
| Wire diameter | 0.50 mm |
| Length | 2 metres |
| Laser welding compatibility | CoCr, compatible dental alloys |
| Use | High-precision laser welding in dental prosthetics |
Delivery
1 roll of Ancordent Cr-Co laser welding wire, 2 m – thickness as selected.